ASTM A213 T24

PropertyDescription
StandardASTM A213 / ASME SA213
GradeT24
UNS NumberK52424
Material TypeFerritic Alloy Steel (2.25Cr–1Mo–0.5W)
Product FormSeamless Tubes
Manufacturing ProcessCold Drawn / Hot Finished
Heat TreatmentNormalized & Tempered
Surface FinishMill Finish, Annealed, Polished
Application TemperatureUp to ~620°C
End FinishesPlain End, Beveled End, Threaded
Categories: , ,

ASTM A213 T24 Seamless Ferritic Alloy Steel Tube

ASTM A213 T24 (UNS K52424) is a high-performance 2.25Cr–1Mo–0.5W ferritic alloy steel tube engineered for high-temperature, high-pressure boiler and superheater systems. This grade provides enhanced creep strength, better oxidation resistance, and improved thermal stability compared to traditional Cr-Mo grades like T22.

T24 is widely used in ultra-supercritical and advanced power plant boilers, refinery furnaces, and heat exchanger systems where long-term durability and resistance to thermal stress are essential.

Key Features

  • High Creep & Stress Rupture Strength
  • Better Oxidation Resistance than T22 due to added tungsten
  • Excellent High-Temperature Performance up to 600–620°C
  • Reduced Wall Thickness Requirement due to improved mechanical strength
  • Superior Resistance to Thermal Fatigue
  • Enhanced Durability for long-life boiler operations
  • Seamless Construction ensures stability under pressure cycling

Equivalent Grades

Standard Equivalent Grade
ASTM A213 T24
UNS K52424
EN / DIN 7CrMoVTiB10-10 (approx.)
ASME SA213 T24
JIS STBA24 (nearest comparable grade)

Available Sizes

  • Outside Diameter (OD): 10 mm – 140 mm
  • Wall Thickness (WT): 1.0 mm – 15 mm
  • Length: 1–12 meters, Custom Cut-to-length
  • Forms: Straight Tubes, U-Bent Tubes, Boiler Coils

ASTM A213 T24 Chemical Composition

Element Content (%)
Carbon (C) 0.05 – 0.10
Manganese (Mn) 0.30 – 0.60
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.010
Silicon (Si) 0.20 – 0.50
Chromium (Cr) 2.20 – 2.60
Molybdenum (Mo) 0.90 – 1.10
Tungsten (W) 0.30 – 0.60
Vanadium (V) 0.20 – 0.30
Niobium (Nb) 0.02 – 0.06
Nitrogen (N) 0.03 – 0.07

ASTM A213 T24 Mechanical Properties

Property Value
Tensile Strength ≥ 590 MPa
Yield Strength (0.2% offset) ≥ 415 MPa
Elongation ≥ 20%
Hardness (HBW) ≤ 250 HB
Impact Energy ≥ 27 J (Room Temperature)

Physical Properties

Property Value
Density 7.80 g/cm³
Thermal Conductivity @ 20°C ~30 W/m·K
Melting Point 1420–1500°C
Electrical Resistivity 0.75 µΩ·m
Modulus of Elasticity 210 GPa
Thermal Expansion Coefficient ~11.5 µm/m°C

Types of ASTM A213 T24 Tubes

  • Seamless Boiler Tubes
  • Superheater Tubes
  • Reheater Tubes
  • Heat Exchanger Tubes
  • U-Bend Tubes
  • High-Pressure Furnace Tubes

Applications

  • Ultra-Supercritical & Supercritical Power Boilers
  • Steam Boilers & Reheater Systems
  • High-Temperature Pressure Equipment
  • Refinery & Petrochemical Furnaces
  • Heat Exchangers & Economizers
  • Thermal Power Plant Components
  • High-Efficiency Boiler Systems

Reviews

There are no reviews yet.

Be the first to review “ASTM A213 T24”

Your email address will not be published. Required fields are marked *

Get A Quote


Please enable JavaScript in your browser to complete this form.
Name

This will close in 0 seconds

Scroll to Top