ASTM A213 TP309

PropertyDescription
StandardASTM A213 / ASME SA213
GradeTP309
UNS NumberS30908
Material TypeAustenitic Stainless Steel
Manufacturing ProcessSeamless (Cold Drawn / Hot Finished)
Delivery ConditionSolution Annealed
Surface FinishAnnealed, Pickled, Bright Annealed
Outer Diameter6 mm – 114 mm
Wall Thickness0.5 mm – 12 mm
LengthUp to 12 meters
Categories: , ,

ASTM A213 TP309 Stainless Steel Tubes (UNS S30908)

ASTM A213 TP309 Stainless Steel Tubes (UNS S30908) are high-temperature austenitic stainless steel tubes designed to deliver excellent oxidation resistance, thermal stability, and mechanical strength in elevated-temperature environments. With high chromium and nickel levels, TP309 withstands temperatures up to 1100°C, making it ideal for furnace parts, superheaters, boilers, heat exchangers, and petrochemical processing.

TP309 is a lower‐carbon version of TP309H, offering good weldability and resistance to thermal shock.

Key Features

  • Excellent oxidation resistance up to 1100°C
  • High chromium & nickel content for thermal stability
  • Superior corrosion resistance in harsh & carburizing atmospheres
  • Good weldability and formability
  • Strong performance in cyclic thermal conditions
  • Ideal for high-temperature continuous service

Equivalent Grade

Standard Grade
UNS S30908
EN / DIN 1.4828 / X15CrNi23-12
JIS SUS 309
GB 12Cr23Ni12
BS 309S
ISO 309

Available Sizes

  • Outside Diameter: 6 mm to 114 mm
  • Wall Thickness: 0.5 mm to 12 mm
  • Length: 1–12 meters (custom available)
  • Forms: Straight, U-bend, Coil-form

ASTM A213 TP309 Chemical Composition

Element Content (%)
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 22.0 – 24.0
Nickel (Ni) 12.0 – 15.0
Nitrogen (N) ≤ 0.10
Iron (Fe) Balance

ASTM A213 TP309 Mechanical Properties

Property Value
Tensile Strength ≥ 620 MPa
Yield Strength (0.2%) ≥ 310 MPa
Elongation (%) ≥ 40
Hardness (HBW) ≤ 192

Physical Properties

Property Value
Density 7.9 g/cm³
Melting Point 1390–1440°C
Thermal Conductivity 14.2 W/m•K
Electrical Resistivity 0.78 μΩ•m
Modulus of Elasticity 200 GPa
Coefficient of Expansion 15.4 μm/m°C

Types of ASTM A213 TP309 Tubes

  • Seamless Stainless Steel Tubes
  • Heat Exchanger Tubes
  • Superheater Tubes
  • Boiler Tubes
  • Reheater Tubes
  • U-Bend Tubes
  • Cold Drawn Tubes
  • Polished Tubes (180–400 Grit)

Applications

  • Industrial Furnaces
  • High-Temperature Boilers
  • Superheaters & Reheaters
  • Heat Exchangers
  • Petrochemical Processing Units
  • Refinery Heaters & Catalytic Cracking
  • Thermal Processing Equipment
  • Exhaust Systems & Burners

Reviews

There are no reviews yet.

Be the first to review “ASTM A213 TP309”

Your email address will not be published. Required fields are marked *

Get A Quote


Please enable JavaScript in your browser to complete this form.
Name

This will close in 0 seconds

Scroll to Top